I needed to push and keep testing my modules till it fails. It sort of did this time. I pushed it to 200A realm and the temperatures went through the roof. Got some Sony VTC5A cells and at the end of the discharge the temps on cells reached 90C which is no no for PETG enclosures. ABS would be better but sure, we don’t want to push cells this hard so they reach 90C. Even 60C is too much if you want your battery pack to last some 🙂
Anyway, here is the video.
I will still do a test later on with LG HB6 cell to see if it stays cooler.